Полиимидная эпоксидная лента is made by polyimide film with imported epoxy modified glue and laminated with paper liner.
Test Item | Unit | Standard | Result | Test way | |
---|---|---|---|---|---|
Color | - | Matt Black | ok | Eye | |
Peel Strength | kgf/cm | ≥0.90 | 0.91-1.13 | IPC-TM6502.4.9 | |
Resin flowability | mm | 0.08-0.18 | 0.09-0.16 | - | |
Insulation resistance | M.D | 1.0×10^11-13 | ok | JIS-C6471.7.1 | |
dimensional stability | MD | % | ≦±0.15 | 0.082 | IPC-TM-6502.2.4 |
TD | % | ≦±0.15 | 0.051 | IPC-TM-6502.2.4 | |
Resistance to immersion welding | % | 300℃/10sec | OK | IPC-TM6502.4.13 | |
Halide Content | ppm | Br≤900 | ok | - | |
CI≤900 | - | ||||
Br+CI≤1500 | - | ||||
Storage conditions | Month | Below 10 ℃,<70% RH | ok | - | |
3 months |
ПРОДУКЦИЯ | Unit | Standard |
---|---|---|
Polymide film Thickness | um | 25±1 |
Epoxy / AD Thickness | um | 25± 2 |
Total Thickness | um | 50± 3 |
Width | mm | 250 /255 /500 |
Length | m | 200 |
Appearance | Number of splicing | ≤3 |
ПРОДУКЦИЯ | Temperature (℃) | Pressure (kgf/cm ²) | Time | |
---|---|---|---|---|
Traditional press | First | 40℃~170℃ | 10 | 45min |
Second | 170℃ | 35 | 45min | |
Third | 170℃~40℃ | 10 | 30min | |
Fast press | 180℃ | 100-120 | Pre pressing for 10s, forming for 100s |
Внимание:На основании приведенной информации и наших советов покупатель самостоятельно определяет соответствие выбранного товара для необходимой ему конкретной цели. За неправильный выбор покупателя компания "Липкая Лента" ответственности не несёт.
Китайский производитель клейких лент по лучшей цене.
Мы предоставляем стандартизированные клейкие ленты и индивидуальные услуги для клиентов из России.
деантапейп Китай © Все права защищены.